Organic-soluble optically transparent polyimides were prepared from alicyclic dianhydride monomer, bicyclo[2.2.2]-oct-7-ene-2,3,5,6-tetracarboxylic dianhydride (BCDA). BCDA gives soluble polyimides with diamines containing at least one flexible linkage such as ether, methylene and sulfide. The polyimides have glass transition temperatures above 350°C and a thermal decomposition temperature of 450°C in an inert atmosphere. The polyimides form a tough film with an ultra-violet cut-off between 300 and 400 nm, which is comparable to that of a fluorinated polyimide.

Посилання на статтю:

Preparation and characterization of organic-soluble optically transparent polyimides from alicyclic dianhydride, bicyclo [ 2.2.2 ] -oct- 7- en e- 2,3,5,6- tetracarboxylic dianhydride / Byong-wa Chun // Polymer. – 1994. – Vol 35. – P. 4203-4208.

Preparation and characterization of organic-soluble optically transparent polyimides from alicyclic dianhydride, bicyclo [ 2.2.2 ] -oct- 7- en e- 2,3,5,6- tetracarboxylic dianhydride - Завантажити.